This article is cited in 3 scientific papers (total in 3 papers)
Thermophysical Properties of Materials
Sintering behavior of mechanically alloyed $\mathrm{Ti}$–$48\mathrm{Al}$–$2\mathrm{Nb}$ aluminides
D. D. Mishra, V. Agarwala, R. C. Agarwala Dept. of Metallurgical and Materials Eng., Indian Institute of Technology Roorkee, Roorkee-247667, India
Abstract:
$\mathrm{Ti}$–$\mathrm{Al}$ intermetallics have been produced using mechanical alloying technique. A composition of $\mathrm{Ti}$–$48\mathrm{Al}$–$2\mathrm{Nb}$ at $\%$ powders was mechanically alloyed for various durations of $20$, $40$, $60$, $80$ and $100$ h. At the early stages of milling, a $\mathrm{Ti (Al)}$ solid solution is formed, on further milling the formation of amorphous phase occurs. Traces of $\mathrm{TiAl}$ and $\mathrm{Ti_3Al}$ were formed with major $\mathrm{Ti}$ and $\mathrm{Al}$ phases after milling at $40$ h and beyond. When further milled, phases of intermetallic compounds like $\mathrm{TiAl}$ and $\mathrm{Ti_3Al}$ were formed after $80$ hours of milling and they also found in $100$ h milled powders. The powders milled for different durations were sintered at $785^\circ$C in vacuum. The mechanically alloyed powders as well as the sintered compacts were characterized by XRD, FESEM and DTA to determine the phases, crystallite size, microstructures and the influence of sintering over mechanical alloying.
Received: 14.02.2013
Citation:
D. D. Mishra, V. Agarwala, R. C. Agarwala, “Sintering behavior of mechanically alloyed $\mathrm{Ti}$–$48\mathrm{Al}$–$2\mathrm{Nb}$ aluminides”, TVT, 52:1 (2014), 71–77; High Temperature, 52:1 (2014), 65–71
Linking options:
https://www.mathnet.ru/eng/tvt9 https://www.mathnet.ru/eng/tvt/v52/i1/p71
|
Statistics & downloads: |
Abstract page: | 182 | Full-text PDF : | 64 | References: | 57 |
|