This article is cited in 16 scientific papers (total in 16 papers)
Lasers
Tunable quasi-cw two-micron lasing in diode-pumped crystals of mixed Tm3+-doped sodium — lanthanum — gadolinium molybdates and tungstates
F. A. Bol'shchikova, E. V. Zharikovb, D. A. Lisb, N. G. Zakharovc, P. A. Ryabochkinaa, K. A. Subbotinb, O. L. Antipovc a Ogarev Mordovia State University
b Prokhorov General Physics Institute of the Russian Academy of Sciences, Moscow
c Institute of Applied Physics, Russian Academy of Sciences, Nizhny Novgorod
Abstract:
Two-micron lasing is obtained for the first time on the 3F4 → 3H6 transition of Tm3+ ions in diode-pumped crystals of mixed sodium — lanthanum — gadolinium tungstate Tm:NaLa1/2Gd1/2(WO4)2 (CTm = 3.6 at %) (3.6Tm : NLGW) and molybdate Tm:NaLa1/3Gd2/3(MoO4)2 (CTm = 4.8 at %) (4.8Tm : NLGM). For the 3.6Tm : NLGW crystal, the quasi-cw laser output power exceeded 200 mW and the slope efficiency (with respect to absorbed pump power) for the π- and σ-polarisations at wavelengths of 1908 and 1918 nm was 34% and 30%, respectively. The laser wavelength of this crystal was continuously tuned within the spectral range of 1860 — 1935 nm. For the 4.8Tm : NLGM crystal, the slope efficiency for the π- and σ-polarisations at wavelengths of 1910 and 1918 nm was 27% and 23%, respectively, and the laser wavelength was tunable within the spectral range of 1870 — 1950 nm.
Received: 21.07.2010 Revised: 27.09.2010
Citation:
F. A. Bol'shchikov, E. V. Zharikov, D. A. Lis, N. G. Zakharov, P. A. Ryabochkina, K. A. Subbotin, O. L. Antipov, “Tunable quasi-cw two-micron lasing in diode-pumped crystals of mixed Tm3+-doped sodium — lanthanum — gadolinium molybdates and tungstates”, Kvantovaya Elektronika, 40:10 (2010), 847–850 [Quantum Electron., 40:10 (2010), 847–850]
Linking options:
https://www.mathnet.ru/eng/qe14403 https://www.mathnet.ru/eng/qe/v40/i10/p847
|
Statistics & downloads: |
Abstract page: | 253 | Full-text PDF : | 108 | References: | 62 | First page: | 1 |
|